Neutron diffraction unveils the ‘relay’ of hardening mechanisms in next-gen superalloys

Neutron diffraction unveils the ‘relay’ of hardening mechanisms in next-gen superalloys











As the aerospace sector pursues propulsion systems that are cleaner, quieter, and more efficient, materials used in turbine components face increasingly demanding thermal and mechanical environments. Ni-Co-based superalloys are widely regarded as prime candidates for next-generation turbine disks due to their exceptional ability to retain strength under extreme temperature and stress.